1. Eliminate work hardening
Source of the problem: During the wire drawing process, metal grains are stretched and deformed, resulting in dislocation accumulation, which leads to increased hardness (work hardening) and decreased ductility.
Annealing solution: Heating to the recrystallization temperature (about 400-600℃ for copper wire and about 700-900℃ for steel wire) reorganizes the grains into an equiaxed structure and restores plasticity.
2. Adjust mechanical properties
Strength control: By adjusting the annealing temperature and time, the tensile strength of the wire can be accurately controlled (such as annealing the copper wire from hard H08 to soft O50).
Case data: After annealing, the elongation of stainless steel wire can be increased from 5% to 35%, meeting the needs of deep processing.
3. Improve surface quality
Oxide layer treatment: Annealing in a protective atmosphere (nitrogen/hydrogen) can reduce the surface copper oxide and make the surface finish of the copper wire Ra≤0.2μm.
Degreasing effect: High temperature decomposes the lubricant remaining in wire drawing to reduce subsequent coating defects.